API-571 practice questions, page 9 of 18, with answer review and explanations.
Question 41
Which API RP recommends programs to monitor small-bore piping, flange faces, blistering and HIC/SOHIC in HF alky units?
574
751
571
980
Question 42
Low creep ductility is __________ severe in high tensile strength materials and welds.
More
Less
Usually
Not
Question 43
_________ is most likely found in hard weld and heat-affected zones and in high strength components.
HIC
SSC
SOHIC
Blistering
Question 44
At elevated temperature, the carbide phases in certain carbon steels are unstable and may decompose into _______. This decomposition is known as graphitization.
Silicon
Graphite nodules
Carbon dust
Graphite dust
Question 45
Hydrogen blisters may form as surface bulges on the ID, the OD on within the wall thickness of a pipe or pressure vessel. Blistering occurs from hydrogen generated by ______, not hydrogen gas from the process stream.