Question 66
If the BHN is 400-500 it may indicate __________.
- Carburization
- Hydriding
- Temper embrittlement
- Caustic embrittlement
Question 67
The graphitization rate ____________ with increasing temperature
- Increases
- Decreases
- Stops
- Proceeds
Question 68
The level of creep damage is a function of the material and the coincident _________ level at which the creep deformation occurs.
- Pressure/Temperature
- Pressure/Stress
- Temperature/Stress
- None of the above
Question 69
Titanium should not be used in known hydriding services such as _____ or ______.
- Caustic, amine
- Amine, sour water
- Sour water, Alkylation
- All of the above
Question 70
Convert these temperatures – 156º C and 450º F
- 304º F, 151º C
- 284º F, 218º C
- 312º F, 232º C
- 296º F, 246º C